speed: 50Hz
15 ml grinding bowl made of tempered steel
+ 2x15 mm Ø temp. steel balls
After 5 minutes of grinding, sample has been comminuted to fine powder. Still longer grinding times are plausible.
To avoid discoloration, we recommend the usage of balls and bowl made of zirconium oxide.